Post by Shawna Richards on Jun 14, 2021 7:13:11 GMT -5
Can I put the original Amazing Clear Cast on my tumbler then use the Quick Coat Epoxy as a second layer?
|
|
|
Post by notoes on Jun 21, 2021 11:05:49 GMT -5
I don't see why not, I've done it on mold box bottoms I've sealed with Amazing Clear Cast and didn't notice any problems.
|
|
|
Post by plzoner on Aug 7, 2021 12:57:09 GMT -5
I am new to the forum. What is the minimum thickness of a pour into a mold using Amazing Clear Cast?
I am trying to duplicate a plastic model windowshield to replace a cracked one. Each pour comes out very flexible. I'm using the included measuring cups with a 50/50 mix. I mix it very thoroughly, pour slowly, curing from 18-24 hours.
I pour in air conditioning but don't heat the mold. Tried that once and destroyed the mold made of regular silicone as it stuck to the part which still turned out flexible.
I'm now using Platt 55 for the mold. I also tried Water Clear which was loaded with bubbles and I don't have a pressure pot.
I'm ready to give up on Alumilite and pitch it all in the trash because I'm spending too much time and it's become too difficult to work with to recreate a small clear part that I can't find without spending more money on a donor kit...for just one part.
|
|
|
Post by Brian on Aug 8, 2021 11:28:17 GMT -5
I'm not sure what the minimal thickness is...I really doubt its anywhere near where you need it to be unless your building in 1/8 or 1/4 scale. There are many builders out there that ditch the kit glass and use piece of clear sheet.....particularly if they want to display it with a partially rolled down window or a hole or holes in the front wind shield. I have also read of builders cutting out what they need from a clear, plastic food container. I have seen many builds using this method...the thickness is more true to scale in 1/25 -1/24 verses the thicker glass in the kits.
|
|