Are there products to create molds that don't require degassing?
|
|
|
Molds
Dec 18, 2015 11:10:00 GMT -5
Post by carol - Alumilite Corp on Dec 18, 2015 11:10:00 GMT -5
Ryan,
Yes the tin cure systems, High Strength series, 1-2 & 3, along with the Quickset do not have to be degassed, you can if you elect to. Most of the platinum cures do need to be deaired because of their viscosity, much thicker.
When using the the High Strength and Quickset to be assured you reduce the chance of any air pockets please see the tutorial on the website. You can brush on a layer of the mixed silicone over the original prior to pouring the silicone to make the mold.
Regards,
Carol