Post by fisheratwork on Nov 18, 2022 9:16:29 GMT -5
Hello, I have a master mold made with PLA+ material, I'm using the VAC MASTER 50 to make the "official" mold, after follow all the instruction this is the resoult: I'm using a wax relase because the spry product was out of stock, brushed with a brush! I think the problem is the density of the mixed part... It's very very dense, this cause a problem if I try to brush with a little brusher on the master mold(to get all the details), and causes flatness problems because it does not adhere at the master mold! My temperature of working is around 15°Celsius, I mixing the part "A" and "B" untill it get soft (5-7minutes) but I notice the part "A" is still verry dense respect to part "B", even if I mix more time the result is the same
|
|