Post by Chofuro on Dec 22, 2021 3:51:13 GMT -5
This is my first time casting molds and parts of my molds (I used Amazing Mold Rubber) are not hardening, I think it is because I didn't shake the catalyst well enough. I made multiple batches, and only the last batch, where I had already reached the bottom of the catalyst cured properly. The rest is wobbly and squishy. I'm pretty sure I used the correct amounts of catalyst... I measured it out with an electronic scale. Will it still cure if I give it time?
|
|
|
Post by notoes on Dec 25, 2021 9:07:36 GMT -5
I'm thinking it might but if it hasn't in a few days, you might want to see if you can add a little extra catalyst to it if it's possible. Sometimes you can just put it on top and it soaks through but sometimes you have to pour it out to add a little extra. If you need more catalyst you can always call Alumilite to get that. Let us know how it comes out.
|
|